Laws of consolidation and homogenization powder steel at its formation by electrocontact compaction (ECC).

Abstract

Laws of consolidation and homogenization powder steel at its formation by electrocontact compaction (ECC).

S.N.Egorov ,T.A. Litvinova,G.A.Shuvaev,H.K.Rizaev

Incoming article date: 12.02.2015

The basic laws of seals and homogenization of powder steel by electrocontact compaction (ECC). Defined process conditions electrocontact compaction (ECC): current density of 36 MA / m², compaction pressure of 380 MPa, the duration of the process 70s that achieve high-density state of the material.

Keywords: electrocontact compaction,zhelezografitovye composition, compactibility, homogenization, porosity, powdered steel, diffusion microstructure splicing current density